Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 84.6 x 10-8 mm³/N-M | 42.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone. Added features of this material include: Internally Lubricated. |
|||
K (wear) Factor | 84.6 x 10-8 mm³/N-M | 42.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC (Asia Pacific) LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Internally Lubricated. |
|||
K (wear) Factor | 84.6 x 10-8 mm³/N-M | 42.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D 3702 Modified |
SABIC Innovative Plastics LNP Lubricomp DP003XXP PC (Europe-Africa-Middle East) LNP* LUBRICOMP* DP003XXP is a compound based on Polycarbonate resin containing PTFE, Silicone. Added features include: Internally Lubricated.This data was supplied by SABIC-IP for the Europe-Africa.. |
|||
K (wear) Factor | 84.6 x 10-8 mm³/N-M | 42.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP WFL36 PBT LNP LUBRICOMP* WFL36 is a compound based on PBT resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
K (wear) Factor | 84.6 x 10-8 mm³/N-M | 42.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP WFL36 PBT (Asia Pacific) LNP LUBRICOMP* WFL36 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
K (wear) Factor | 84.6 x 10-8 mm³/N-M | 42.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP WFL36 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WFL36 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE. |