Mechanical Properties Metric English Comments
K (wear) Factor 127 - 179 x 10-8 mm³/N-M
63.0 - 89.0 x 10-10 in³-min/ft-lb-hr
Average value: 148 x 10<sup>-8</sup> mm³/N-M Grade Count:5
Overview of materials for Acetal Copolymer, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va..
K (wear) Factor 127 x 10-8 mm³/N-M
63.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D 3702 Modified
SABIC Innovative Plastics LNP Lubricomp KCL34 Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KCL34 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data ..
K (wear) Factor 127 x 10-8 mm³/N-M
63.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D 3702 Modified
SABIC Innovative Plastics LNP Lubricomp QCL329 PA 6/10
LNP LUBRICOMP* QCL329 is a compound based on Nylon 6/10 resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was supplied..
K (wear) Factor 127 x 10-8 mm³/N-M
63.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D 3702 Modified
SABIC Innovative Plastics LNP Lubricomp QCL329 PA 6/10 (Asia Pacific)
LNP LUBRICOMP* QCL329 is a compound based on Nylon 6/10 resin containing Carbon Fiber, PTFE, Flame Retardant. Added features of this material include: Electrically Conductive.This data was supplied..
K (wear) Factor 127 x 10-8 mm³/N-M
63.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D 3702 Modified
SABIC Innovative Plastics LNP Lubricomp KCL34 Acetal Copoly
LNP* Lubricomp* KCL34 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data ..
K (wear) Factor 127 x 10-8 mm³/N-M
63.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D 3702 Modified
SABIC Innovative Plastics LNP Lubricomp KCL36 Acetal Copoly
LNP* Lubricomp* KCL36 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data ..
K (wear) Factor 127 x 10-8 mm³/N-M
63.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP KCL36 Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KCL36 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.
K (wear) Factor 127 x 10-8 mm³/N-M
63.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP STAT-KON QEL329 PA 6/10
LNP STAT-KON* QEL329 is a compound based on Nylon 6/10 resin containing 10% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant, Flame Retardant..
K (wear) Factor 127 x 10-8 mm³/N-M
63.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP STAT-KON QEL329 PA 6/10 (Asia Pacific)