Polymer Property : K (wear) Factor = 8.80 x 10-8 mm³/N-M Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 8.80 x 10-8 mm³/N-M
4.37 x 10-10 in³-min/ft-lb-hr
LATI Latilub 80-15T K/30 PPS, 30% Carbon Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati ..