Polymer Property : Tensile Strength, Yield = 1070 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 7.35 MPa

@Strain 5.00 %
1070 psi

@Strain 5.00 %
ASTM D638
SK Chemicals SKYPEL G155D General Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Tensile Strength, Yield 7.35 MPa

@Strain 10.0 %
1070 psi

@Strain 10.0 %
ASTM D638
SK Chemicals SKYPEL P147D Productivity Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Tensile Strength, Yield 7.35 MPa

@Strain 300 %
1070 psi

@Strain 300 %
ASTM D412
SK Chemicals SKYTHANE® 875A T series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tensile Strength, Yield 7.35 MPa

@Strain 100 %
1070 psi

@Strain 100 %
ASTM D412
SK Chemicals SKYTHANE® 585A X series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..