Mechanical Properties Metric English Comments
Tensile Strength, Yield 75.2 MPa

@Temperature 150 °C
10900 psi

@Temperature 302 °F
Conditioned; ISO 527-2
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)  (Unverified Data**)
Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar..
Tensile Strength, Yield 75.2 MPa

@Temperature 150 °C
10900 psi

@Temperature 302 °F
ISO 527-2
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)  (Unverified Data**)
Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar..
Tensile Strength, Yield 75.2 MPa

@Temperature 23.0 °C
10900 psi

@Temperature 73.4 °F
ISO 527-2
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and better ..
Tensile Strength, Yield 75.0 MPa

@Temperature 100 °C
10900 psi

@Temperature 212 °F
ASTM D638
Gharda Chemicals G-PAEKâ„¢ 1200G Ultra High Performance PEK Polymer
Product Details: Ultra High Performance Thermoplastic (Poly Aryl Ether Ketone) material, virgin semi-crystalline granules suitable for injection molding, easy flow, Beige in colorApplication Areas:..
Tensile Strength, Yield 75.0 MPa

@Temperature 250 °C
10900 psi

@Temperature 482 °F
ASTM D638
Gharda Chemicals G-PAEKâ„¢ 1230CF Ultra High Performance PEK Polymer
Product Details: Ultra High Performance Thermoplastic material, 30% carbon fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, easy flow, Black in ..
Tensile Strength, Yield 75.2 MPa

@Thickness 1.57 mm
10900 psi

@Thickness 0.0620 in
CW; ASTM D638
Industrial Laminates/Norplex NP342 Cotton Fabric
Description: Fine weave canvas phenolic material with fabric construction weight intermediate to NP310 and NP320. Designed for better machining than grade NP310 and lower cost than NP320.Thickness T..
Tensile Strength, Yield 75.0 MPa

@Strain 0.200 %,
Temperature 1000 °C
10900 psi

@Strain 0.200 %,
Temperature 1830 °F
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Age-hardened
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Tensile Strength, Yield 75.2 MPa

@Temperature 150 °C
10900 psi

@Temperature 302 °F
4; ISO 527-2
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Conditioned)
Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in..
Tensile Strength, Yield 75.2 MPa

@Temperature 150 °C
10900 psi

@Temperature 302 °F
4; ISO 527-2
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in..
Tensile Strength, Yield 75.2 MPa

@Temperature 23.0 °C
10900 psi

@Temperature 73.4 °F
2; ISO 527-2
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)
Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet..
Tensile Strength, Yield 75.2 MPa

@Temperature 93.3 °C
10900 psi

@Temperature 200 °F
90°, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, AS4 Fiber
Information provided by HexCel
Tensile Strength, Yield 75.0 MPa

@Strain 0.200 %,
Temperature 1000 °C
10900 psi

@Strain 0.200 %,
Temperature 1830 °F
Haynes 282® Nickel Alloy Plate, Solution Annealed and Age-Hardened