Polymer Property : Tensile Strength, Yield = 13.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 13.0 MPa

@Strain 300 %
1890 psi

@Strain 300 %
ASTM D412
GRECO ISOTHANE 2058A Poly(caprolactone)ester TPU Resin
ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stabi..
Tensile Strength, Yield 13.0 MPa

@Strain 50.0 %
1890 psi

@Strain 50.0 %
ASTM D412
GRECO ISOTHANE 3055D Polyether TPU Resin
ISOTHANE 3000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These prod..
Tensile Strength, Yield 13.0 MPa

@Strain 300 %
1890 psi

@Strain 300 %
ASTM D412
GRECO ISOTHANE 1085AF Poly(adipate)ester TPU Resin
ISOTHANE 1000 FDA series products are poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance and solvent resistance. These products can be inject..
Tensile Strength, Yield 13.0 MPa

@Strain 50.0 %
1890 psi

@Strain 50.0 %
ASTM D412
GRECO ISOTHANE 1170D Poly(adipate)ester TPU Resin
ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp..
Tensile Strength, Yield 13.0 MPa

@Strain 100 %
1890 psi

@Strain 100 %
ASTM D-412
BASF Elastollan® C-95A Polyester Type Polyurethane Elastomer
Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen..