GRECO ISOTHANE 1085AF Poly(adipate)ester TPU Resin

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer GRECO
Trade Name ISOTHANE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF GRECO ISOTHANE 1085AF Poly(adipate)ester TPU Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ISOTHANE 1000 FDA series products are poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance and solvent resistance. These products can be injection molded, blow molded, and extruded. In compliance with FDA CFR 177.105, 177.1680, and 177.2600 requirementsInformation provided by Greater Eastern Resins Industrial Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
ASTM D2240
Tensile Strength 36.0 MPa
5220 psi
ASTM D412
Tensile Strength, Yield 4.10 MPa

@Strain 50.0 %
595 psi

@Strain 50.0 %
ASTM D412
6.20 MPa

@Strain 100 %
899 psi

@Strain 100 %
ASTM D412
13.0 MPa

@Strain 300 %
1890 psi

@Strain 300 %
ASTM D412
Elongation at Break 580 %
580 %
ASTM D412
Tear Strength 80.0 kN/m
456 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 20
20
ASTM D1044(Taber) H-22
Compression Set 25 %

@Temperature 23.0 °C,
Time 79200 sec
25 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
75 %

@Temperature 70.0 °C,
Time 79200 sec
75 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395