Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1482 MPa @Temperature 71.0 °C |
214900 psi @Temperature 160 °F |
1/2 hr |
Hexcel® F515 Epoxy Resin, TXX200 Carbon Tape STD MOD FiberInformation provided by HexCel |