Mechanical Properties Metric English Comments
Tensile Strength, Yield 1790 MPa

@Strain 0.200 %
260000 psi

@Strain 0.200 %
hardened to 50 RC
Bohler-Uddeholm UDDEHOLM ELMAX® Powder Metallurgy Stainless Mold Steel
High chromium-vanadium-molybdenum alloyed steelA through-hardening corrosion resistant mold steel made by powder metallurgy processing techniques. The high wear resistance makes ELMAX® suitable for..
Tensile Strength, Yield 1790 MPa

@Strain 0.200 %
260000 psi

@Strain 0.200 %
hardness of 52 HRC
Bohler-Uddeholm UDDEHOLM HOTVAR® Hot Work Tool Steel
Molybdenum-vanadium alloyed steelHotvar® is a premium hot work steel developed by Uddeholm to provide very good performance in tooling up to 1200°F (650°C). The alloying elements in Hotvar® are ..