Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1790 MPa @Strain 0.200 % |
260000 psi @Strain 0.200 % |
hardened to 50 RC |
Bohler-Uddeholm UDDEHOLM ELMAX® Powder Metallurgy Stainless Mold Steel High chromium-vanadium-molybdenum alloyed steelA through-hardening corrosion resistant mold steel made by powder metallurgy processing techniques. The high wear resistance makes ELMAX® suitable for.. |
|||
Tensile Strength, Yield | 1790 MPa @Strain 0.200 % |
260000 psi @Strain 0.200 % |
hardness of 52 HRC |
Bohler-Uddeholm UDDEHOLM HOTVAR® Hot Work Tool Steel Molybdenum-vanadium alloyed steelHotvar® is a premium hot work steel developed by Uddeholm to provide very good performance in tooling up to 1200°F (650°C). The alloying elements in Hotvar® are .. |