Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 182 MPa @Temperature 200 °C |
>= 26400 psi @Temperature 392 °F |
|
PEAK Werkstoff DISPAL S541 Aluminum Alloy, AlMg6Mn4SiTiZr, Condition F Information provided by PEAK Werkstoff GmbH |
|||
Tensile Strength, Yield | 182 MPa @Temperature 759 °C |
26400 psi @Temperature 1400 °F |
Autogenously Welded plate, 1.6mm thick |
Special Metals INCOLOY® alloy 864 INCOLOY® alloy 8684 (UNS S35135) was specifically developed for automotive exhaust system flexible couplings, EGR tubes, manifolds and tailpipes. It exhibits excellent fatigue resistance, therma.. |
|||
Tensile Strength, Yield | 182 MPa @Strain 0.200 %, Temperature 260 °C |
26400 psi @Strain 0.200 %, Temperature 500 °F |
Plate |
AK Steel NITRONIC® 30 Austenitic Stainless Steel AK Steel NITRONIC 30 Stainless Steel offers significantly higher strength than Type 304 and potential for applications requiring good resistance to aqueous and atmospheric corrosion resistance combi.. |