Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 156 MPa @Strain 1.00 %, Temperature 400 °C |
22600 psi @Strain 1.00 %, Temperature 752 °F |
EN min.; EN 10002-5 |
Outokumpu 4311 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Tensile Strength, Yield | 156 MPa @Strain 1.00 %, Temperature 300 °C |
22600 psi @Strain 1.00 %, Temperature 572 °F |
EN min.; EN 10002-5 |
Outokumpu 4404 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Yield | 156 MPa @Strain 1.00 %, Temperature 300 °C |
22600 psi @Strain 1.00 %, Temperature 572 °F |
EN min.; EN 10002-5 |
Outokumpu 4432 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Yield | 156 MPa @Strain 1.00 %, Temperature 400 °C |
22600 psi @Strain 1.00 %, Temperature 752 °F |
EN min.; EN 10002-5 |
Outokumpu 4541 Cr-Ni Austenitic Stainless Steel Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto), hot rolled strip/sheet (C.. |
|||
Tensile Strength, Yield | 156 MPa @Temperature 649 °C |
22600 psi @Temperature 1200 °F |
ASTM E8 |
ATI Allegheny Ludlum 310 Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |