Mechanical Properties Metric English Comments
Tensile Strength, Yield 157 MPa

@Strain 1.00 %,
Temperature 200 °C
22800 psi

@Strain 1.00 %,
Temperature 392 °F
EN min.; EN 10002-5
Outokumpu 4301 Cr-Ni Austenitic Stainless Steel
General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll..
Tensile Strength, Yield 157 MPa

@Strain 0.200 %,
Temperature 100 °C
22800 psi

@Strain 0.200 %,
Temperature 212 °F
EN min.; EN 10002-5
Outokumpu 4301 Cr-Ni Austenitic Stainless Steel
General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll..
Tensile Strength, Yield 157 MPa

@Strain 0.200 %,
Temperature 200 °C
22800 psi

@Strain 0.200 %,
Temperature 392 °F
EN min.; EN 10002-5
Outokumpu 4311 Cr-Ni Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms..
Tensile Strength, Yield 157 MPa

@Strain 0.200 %,
Temperature 200 °C
22800 psi

@Strain 0.200 %,
Temperature 392 °F
EN min.; EN 10002-5
Outokumpu 4541 Cr-Ni Austenitic Stainless Steel
Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto), hot rolled strip/sheet (C..
Tensile Strength, Yield 157 MPa

@Strain 0.200 %,
Temperature 200 °C
22800 psi

@Strain 0.200 %,
Temperature 392 °F
EN min.; EN 10002-5
Outokumpu 4550 Austenitic Stainless Steel
Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto) and rod forms.
Tensile Strength, Yield 157 MPa

@Strain 0.200 %,
Temperature 427 °C
22800 psi

@Strain 0.200 %,
Temperature 800 °F
Plate
AK Steel NITRONIC® 30 Austenitic Stainless Steel
AK Steel NITRONIC 30 Stainless Steel offers significantly higher strength than Type 304 and potential for applications requiring good resistance to aqueous and atmospheric corrosion resistance combi..
Tensile Strength, Yield 157 MPa

@Strain 1.00 %,
Temperature 200 °C
22800 psi

@Strain 1.00 %,
Temperature 392 °F
EN min.; EN 10002-5
Outokumpu 4948 High Temperature Austenitic Stainless Steel
Creep-resistant variant of 1.4301, with a standardized minimum carbon content for service at temperatures of up to 800°C in dry air.Applications: Heat and creep resistance. For use over 550°C for..
Tensile Strength, Yield 157 MPa

@Strain 0.200 %,
Temperature 100 °C
22800 psi

@Strain 0.200 %,
Temperature 212 °F
EN min.; EN 10002-5
Outokumpu 4948 High Temperature Austenitic Stainless Steel
Creep-resistant variant of 1.4301, with a standardized minimum carbon content for service at temperatures of up to 800°C in dry air.Applications: Heat and creep resistance. For use over 550°C for..