Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 3.70 MPa @Strain 50.0 % |
537 psi @Strain 50.0 % |
ASTM D412 |
GRECO ISOTHANE 1080A Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products .. |
|||
Tensile Strength, Yield | 3.70 MPa @Strain 50.0 % |
537 psi @Strain 50.0 % |
ASTM D412 |
GRECO ISOTHANE 2080A Poly(caprolactone)ester TPUÂ Resin ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stabi.. |