Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 3.70 MPa

@Strain 50.0 %
537 psi

@Strain 50.0 %
ASTM D412
GRECO ISOTHANE 1080A Poly(adipate)ester TPU Resin
ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products ..
Tensile Strength, Yield 3.70 MPa

@Strain 50.0 %
537 psi

@Strain 50.0 %
ASTM D412
GRECO ISOTHANE 2080A Poly(caprolactone)ester TPU Resin
ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stabi..