Polymer Property : Tensile Strength, Yield = 30600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 211 MPa

@Strain 1.00 %,
Temperature 100 °C
30600 psi

@Strain 1.00 %,
Temperature 212 °F
EN min.; EN 10002-5
Outokumpu 4404 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Tensile Strength, Yield 211 MPa

@Strain 0.200 %,
Temperature 100 °C
30600 psi

@Strain 0.200 %,
Temperature 212 °F
EN min.; EN 10002-5
Outokumpu 4406 Cr-Ni-Mo Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms..
Tensile Strength, Yield 211 MPa

@Strain 0.200 %,
Temperature 100 °C
30600 psi

@Strain 0.200 %,
Temperature 212 °F
EN min.; EN 10002-5
Outokumpu 4429 Cr-Ni-Mo Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), cold rolled strip/sheet and rod forms.
Tensile Strength, Yield 211 MPa

@Strain 1.00 %,
Temperature 100 °C
30600 psi

@Strain 1.00 %,
Temperature 212 °F
EN min.; EN 10002-5
Outokumpu 4432 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Tensile Strength, Yield 211 MPa

@Thickness 9.50 mm,
Temperature 760 °C
30600 psi

@Thickness 0.374 in,
Temperature 1400 °F
0.2% offset
Haynes Hastelloy® C-4 alloy, plate, heat treated at 1066°C, rapid quenched
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang..