Mechanical Properties Metric English Comments
Tensile Strength, Yield 344 MPa

@Strain 0.200 %,
Temperature 540 °C
49900 psi

@Strain 0.200 %,
Temperature 1000 °F
AMS 5879
Haynes 625SQ® Nickel Alloy Sheet
Haynes 625SQ alloy is a solid-solution strengthened superalloy. It is a modification of Haynes 625 alloy designed to enhance resistance to fatigue at temperatures up to approximately 1200°F (649Â..
Tensile Strength, Yield 344 MPa

@Thickness 6.40 mm,
Temperature 25.0 °C
49900 psi

@Thickness 0.252 in,
Temperature 77.0 °F
0.2% Offset
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2075°F (1135°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..