Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 344 MPa @Strain 0.200 %, Temperature 540 °C |
49900 psi @Strain 0.200 %, Temperature 1000 °F |
AMS 5879 |
Haynes 625SQ® Nickel Alloy Sheet Haynes 625SQ alloy is a solid-solution strengthened superalloy. It is a modification of Haynes 625 alloy designed to enhance resistance to fatigue at temperatures up to approximately 1200°F (649Â.. |
|||
Tensile Strength, Yield | 344 MPa @Thickness 6.40 mm, Temperature 25.0 °C |
49900 psi @Thickness 0.252 in, Temperature 77.0 °F |
0.2% Offset |
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |