Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 360 MPa @Strain 0.200 %, Temperature 100 °C |
52200 psi @Strain 0.200 %, Temperature 212 °F |
EN min.; EN 10002-5 |
Outokumpu 2205 Duplex Stainless Steel Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical t.. |
|||
Tensile Strength, Yield | 360 MPa @Strain 0.200 % |
52200 psi @Strain 0.200 % |
Outokumpu Typical,Hot rolled Strip/Sheet (CPP); EN 10002-1 |
Outokumpu 353MA® High Temperature Austenitic Stainless Steel Alloy with higher nickel content than the other steels. Has increased silicon and nitrogen contents and is microalloyed with rare earth metals (REM). Max service temperature in air is 1150°C, but.. |
|||
Tensile Strength, Yield | 360 MPa @Strain 1.00 % |
52200 psi @Strain 1.00 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4311 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Tensile Strength, Yield | 360 MPa @Strain 0.200 % |
52200 psi @Strain 0.200 % |
Outokumpu Typical,Cold Rolled Strip/Sheet; EN 10002-1 |
Outokumpu 4318 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled strip/sheet (CPP) and cold rolled strip sheet forms. |
|||
Tensile Strength, Yield | 360 MPa @Strain 1.00 % |
52200 psi @Strain 1.00 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4406 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Tensile Strength, Yield | 360 MPa @Strain 0.200 % |
52200 psi @Strain 0.200 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4529 Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form. |
|||
Tensile Strength, Yield | 360 MPa @Thickness 3.20 mm, Temperature 93.0 °C |
52200 psi @Thickness 0.126 in, Temperature 199 °F |
0.2% Offset |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Sheet, Cold Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Tensile Strength, Yield | >= 360 MPa @Strain 2.00 % |
>= 52200 psi @Strain 2.00 % |
bake hardening after 2% strain and heating to 170°C for 20 min. |
SSAB Tunnplat Docol® 300 BH High-strength Steel High-strength SteelComments: Docol BH - Cold Rolled Steel - rephosphorized steel with bake hardening effect. Property values are for cold-rolled steel; thicknesses 0.40 - 2.0 mm. Iron content is ap.. |
|||
Tensile Strength, Yield | 360 MPa @Strain 0.200 %, Thickness 127 - 152.4 mm |
52200 psi @Strain 0.200 %, Thickness 5.00 - 6.000 in |
Typical Strength |
Constellium Alumold® 350 Aluminum Alumold-350® has been specifically developed to achieve the best combination of strength at low and high temperatures, together with a good shape stability and machinability. Alumold-350® is parti.. |
|||
Tensile Strength, Yield | 360 MPa @Strain 0.200 %, Thickness 203.2 - 254 mm |
52200 psi @Strain 0.200 %, Thickness 8.000 - 10.0 in |
Typical Strength |
Constellium Alumold® 400 Aluminum The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds.. |
|||
Tensile Strength, Yield | 360 MPa @Strain 0.200 %, Thickness 60.0 - 80.0 mm |
52200 psi @Strain 0.200 %, Thickness 2.36 - 3.15 in |
Typical Strength |
Constellium Unidal® High-Strength Rolled Precision Aluminum Plate, Milled Both Sides Unidal® precision plates offers a combination of dimensional stability and high mechanical strength. The very low internal stress reduces the risk of deformation during machining, thereby reducing .. |