SSAB Tunnplat Docol® 300 BH High-strength Steel

Category Metal , Ferrous Metal , Alloy Steel , Low Alloy Steel
Manufacturer SSAB Tunnplat AB
Trade Name Docol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SSAB Tunnplat Docol® 300 BH High-strength Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High-strength SteelComments: Docol BH - Cold Rolled Steel - rephosphorized steel with bake hardening effect. Property values are for cold-rolled steel; thicknesses 0.40 - 2.0 mm. Iron content is approximate - exact composition is not reported by the manufacturer.Data provided by SSAB Tunnplat.
Physical Properties Metric English Comments
Density 7.87 g/cc
0.284 lb/in³
Estimated by MatWeb
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 420 - 500 MPa
60900 - 72500 psi
Tensile Strength, Yield 300 - 360 MPa

@Strain 0.200 %
43500 - 52200 psi

@Strain 0.200 %
>= 360 MPa

@Strain 2.00 %
>= 52200 psi

@Strain 2.00 %
bake hardening after 2% strain and heating to 170°C for 20 min.
Elongation at Break >= 26 %
>= 26 %
A<sub>80</sub>
Component Elements Properties Metric English Comments
Iron, Fe 98 %
98 %