Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 440 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 440 MPa

@Strain 0.200 %
63800 psi

@Strain 0.200 %
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 4565 High Performance Austenitic Stainless Steel
Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar..
Tensile Strength, Yield 440 MPa

@Strain 1.00 %
63800 psi

@Strain 1.00 %
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 4762 High Temperature Ferritic Stainless Steel
Highest chromium content-most resistant to reducing sulphurous gases. Susceptible to 475°C embrittlement and s-phase forms during long exposures in the range 600-800°C.Applications: Mostly used i..
Tensile Strength, Yield >= 440 MPa

@Strain 1.00 %
>= 63800 psi

@Strain 1.00 %
Industeel URANUS® 35N 23.04 Duplex Stainless Steel with PREN = 24
Description: URANUS® 35N (UR 35N) is a 23% Cr, 4% Nickel, Mo free duplex stainless steel (23.04). The alloy UR 35N has similar corrosion resistance properties similar to 316L. Furthermore, its me..
Tensile Strength, Yield >= 440 MPa

@Strain 1.00 %
>= 63800 psi

@Strain 1.00 %
Industeel URANUS® B66 High Strength Super-Austenitic Stainless Steel with PREN = 54
Description: Research carried out these last five years has shown that combined additions of chromium, tungsten, molybdenum, nitrogen and copper, make it possible to design a super-austenitic stainl..
Tensile Strength, Yield >= 440 MPa

@Strain 0.200 %,
Temperature 300 °C
>= 63800 psi

@Strain 0.200 %,
Temperature 572 °F
ThyssenKrupp N-A-XTRA® 550 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..
Tensile Strength, Yield >= 440 MPa

@Strain 0.200 %,
Thickness 50.0 - 60.0 mm
>= 63800 psi

@Strain 0.200 %,
Thickness 1.97 - 2.36 in
Temper T651; Standard EN 485-2
Constellium ALPLAN® 7075 High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
ALPLAN® 7075 precision plates combine a good dimensional stability with high mechanical strength. Both the outstanding flatness and the low roughness of the surfaces, protected by a plastic film, m..
Tensile Strength, Yield >= 440 MPa

@Strain 0.200 %,
Thickness 150 - 240 mm
>= 63800 psi

@Strain 0.200 %,
Thickness 5.91 - 9.45 in
Tempers T651 / T652
Constellium Certal® SPC Aluminum
Certal® SPC has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property in man..
Tensile Strength, Yield >= 440 MPa

@Diameter 63.0 mm
>= 63800 psi

@Diameter 2.48 in
Re. Core strength in hardened condition.
Assab Steels 7210M Machinery Steel
ASSAB 7210M is an alloyed case hardening steel with high core strength.Applications: ASSAB 7210M is used for applications requiring a hard, wear resistant surface and a tough core, such as transmiss..