Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Industeel URANUS® 35N 23.04 Duplex Stainless Steel with PREN = 24

Category Metal , Ferrous Metal , Duplex , Stainless Steel , T S30000 Series Stainless Steel
Manufacturer Groupe Arcelor
Trade Name URANUS®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Industeel URANUS® 35N 23.04 Duplex Stainless Steel with PREN = 24.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: URANUS® 35N (UR 35N) is a 23% Cr, 4% Nickel, Mo free duplex stainless steel (23.04). The alloy UR 35N has similar corrosion resistance properties similar to 316L. Furthermore, its mechanical properties i.e. yield strength, are twice those of 304/316 austenitic grades. This allows the designer to save weight, particularly for properly designed pressure vessel applications. The alloy is particularly suitable for applications covering the -50°C/+300°C (-58°F/572°F) temperature range. Lower temperatures may also be considered, but need some restrictions, particularly for welded structures. With its duplex microstructure, low nickel and high chromium contents, the alloy has improved stress corrosion resistance properties compared to 304 and 316 austenitic grades.Information provided by manufacturer.
Physical Properties Metric English Comments
Density 7.80 g/cc
0.282 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 180 - 230
180 - 230
Typical
Hardness, Rockwell C <= 20
<= 20
Typical
Tensile Strength, Ultimate >= 600 MPa
>= 87000 psi
Tensile Strength, Yield >= 400 MPa

@Strain 0.200 %
>= 58000 psi

@Strain 0.200 %
>= 440 MPa

@Strain 1.00 %
>= 63800 psi

@Strain 1.00 %
Elongation at Break >= 25 %
>= 25 %
Modulus of Elasticity 200 GPa
29000 ksi
Poissons Ratio 0.333
0.333
Calculated
Shear Modulus 75.0 GPa

@Temperature 20.0 °C
10900 ksi

@Temperature 68.0 °F
Charpy Impact >= 90.0 J
>= 66.4 ft-lb
150 J
111 ft-lb
Typical
>= 75.0 J

@Temperature -50.0 °C
>= 55.3 ft-lb

@Temperature -58.0 °F
90.0 J

@Temperature -50.0 °C
66.4 ft-lb

@Temperature -58.0 °F
Typical
Thermal Properties Metric English Comments
CTE, linear 13.0 µm/m-°C

@Temperature 20.0 - 100 °C
7.22 µin/in-°F

@Temperature 68.0 - 212 °F
13.5 µm/m-°C

@Temperature 20.0 - 200 °C
7.50 µin/in-°F

@Temperature 68.0 - 392 °F
14.0 µm/m-°C

@Temperature 20.0 - 300 °C
7.78 µin/in-°F

@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.450 J/g-°C

@Temperature 20.0 °C
0.108 BTU/lb-°F

@Temperature 68.0 °F
Thermal Conductivity 17.0 W/m-K

@Temperature 20.0 °C
118 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Component Elements Properties Metric English Comments
Carbon, C 0.020 %
0.020 %
Chromium, Cr 23 %
23 %
Iron, Fe 72.679 %
72.679 %
As remainder
Molybdenum, Mo 0.20 %
0.20 %
Nickel, Ni 4.0 %
4.0 %
Nitrogen, N 0.10 %
0.10 %
Sulfur, S 0.0010 %
0.0010 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000800 ohm-cm

@Temperature 20.0 °C
0.0000800 ohm-cm

@Temperature 68.0 °F