Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 465 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 465 MPa

@Thickness 12.7 mm,
Temperature 25.0 °C
67400 psi

@Thickness 0.500 in,
Temperature 77.0 °F
0.2% offset
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Tensile Strength, Yield 465 MPa

@Strain 0.200 %,
Thickness 12.7 mm
67400 psi

@Strain 0.200 %,
Thickness 0.500 in
as welded
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Tensile Strength, Yield 465 MPa

@Strain 0.200 %,
Thickness 60.0 - 80.0 mm
67400 psi

@Strain 0.200 %,
Thickness 2.36 - 3.15 in
Typical Strength
Constellium ALPLAN® 7075 High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
ALPLAN® 7075 precision plates combine a good dimensional stability with high mechanical strength. Both the outstanding flatness and the low roughness of the surfaces, protected by a plastic film, m..
Tensile Strength, Yield 465 MPa

@Strain 0.200 %,
Thickness 120 - 140 mm
67400 psi

@Strain 0.200 %,
Thickness 4.72 - 5.51 in
Typical Strength
Constellium Fortal® Aluminum Alloy
Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m..
Tensile Strength, Yield 465 MPa

@Strain 0.200 %
67400 psi

@Strain 0.200 %
Transverse
AK Steel ULTRALUME® Press Hardenable Carbon Steel
ULTRALUME Press Hardenable Steel (PHS) is AK Steel’s newest addition to our expanding product portfolio of Advanced High Strength Steels (AHSS). Aluminized Type 1 ULTRALUME PHS is intended for auto..
Copyright © lookpolymers.com All Rights Reserved