Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 465 MPa @Thickness 12.7 mm, Temperature 25.0 °C |
67400 psi @Thickness 0.500 in, Temperature 77.0 °F |
0.2% offset |
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Tensile Strength, Yield | 465 MPa @Strain 0.200 %, Thickness 12.7 mm |
67400 psi @Strain 0.200 %, Thickness 0.500 in |
as welded |
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Tensile Strength, Yield | 465 MPa @Strain 0.200 %, Thickness 60.0 - 80.0 mm |
67400 psi @Strain 0.200 %, Thickness 2.36 - 3.15 in |
Typical Strength |
Constellium ALPLAN® 7075 High-Strength Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 7075 precision plates combine a good dimensional stability with high mechanical strength. Both the outstanding flatness and the low roughness of the surfaces, protected by a plastic film, m.. |
|||
Tensile Strength, Yield | 465 MPa @Strain 0.200 %, Thickness 120 - 140 mm |
67400 psi @Strain 0.200 %, Thickness 4.72 - 5.51 in |
Typical Strength |
Constellium Fortal® Aluminum Alloy Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m.. |
|||
Tensile Strength, Yield | 465 MPa @Strain 0.200 % |
67400 psi @Strain 0.200 % |
Transverse |
AK Steel ULTRALUME® Press Hardenable Carbon Steel ULTRALUME Press Hardenable Steel (PHS) is AK Steel’s newest addition to our expanding product portfolio of Advanced High Strength Steels (AHSS). Aluminized Type 1 ULTRALUME PHS is intended for auto.. |