Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 485 MPa @Strain 0.200 %, Temperature 350 °C |
>= 70300 psi @Strain 0.200 %, Temperature 662 °F |
|
ThyssenKrupp N-A-XTRA® 620 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Tensile Strength, Yield | 485 MPa @Temperature -54.0 °C |
70300 psi @Temperature -65.2 °F |
Dry |
Hexcel® HexPly® F593 Epoxy Resin, W3G282 Carbon Fabric Hexcel designation: W3G282-42"-F593; Fiber: Amoco T-300/3kInformation provided by HexCel |
|||
Tensile Strength, Yield | 485 MPa @Strain 0.200 %, Thickness 50.0 - 60.0 mm |
70300 psi @Strain 0.200 %, Thickness 1.97 - 2.36 in |
Typical Strength |
Constellium Fortal® Aluminum Alloy Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m.. |
|||
Tensile Strength, Yield | 485 MPa @Strain 0.200 % |
70300 psi @Strain 0.200 % |
Typical |
Aleris Hokotol Aluminum Alloy, 200 mm Thickness Sample treatment not specified for property data.Applications include molds for blow forming and injection molding for plastics; bolsters and force plates; high strength/low weight machine parts; an.. |