Mechanical Properties Metric English Comments
Tensile Strength, Yield 49.0 MPa

@Temperature 23.0 °C
7110 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® ST801AW NC010 Nylon 66  (Unverified Data**)
Zytel® ST801AW NC010 is a Super Tough, high performance polyamide 66 resin. It is UV stabilized and when appropriately colored offers the best resistance to indirect sunlight in automotive interior..
Tensile Strength, Yield 49.0 MPa

@Thickness 3.20 mm
7110 psi

@Thickness 0.126 in
Type I, 50 mm/min; ASTM D638
Bhansali Engineering Abstron TG3MM ABS Injection Molding Grade
Medium Flow, Medium Impact, high RigidityInformation provided by Bhansali
Tensile Strength, Yield 49.0 MPa

@Thickness 3.20 mm
7110 psi

@Thickness 0.126 in
Type I, 50 mm/min; ASTM D638
Bhansali Engineering Abstron TG3MM ABS Injection Molding Grade
Medium Flow, Medium Impact, high RigidityInformation provided by Bhansali
Tensile Strength, Yield 49.0 MPa

@Strain 0.200 %,
Temperature 704 °C
7110 psi

@Strain 0.200 %,
Temperature 1300 °F
AK Steel 439 ULTRA FORM® Stainless Steel
AK Steel 439 ULTRA FORM™ was developed for applications requiring oxidation and corrosion resistance superior to Type 409 as well as superior formability to AK Steel 439 Stainless Steel. As a resul..