Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 520 MPa @Strain 0.200 %, Temperature 250 °C |
>= 75400 psi @Strain 0.200 %, Temperature 482 °F |
|
ThyssenKrupp N-A-XTRA® 620 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Tensile Strength, Yield | 520 MPa @Strain 0.200 % |
75400 psi @Strain 0.200 % |
after porcelain firing |
Wieland Duo Pal 6 PFM Alloy Palladium-base ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials, ceramic veneering, acrylic veneeringDental |
|||
Tensile Strength, Yield | 520 MPa @Strain 0.200 % |
75400 psi @Strain 0.200 % |
hardened |
Wieland Duo Pal 6 PFM Alloy Palladium-base ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials, ceramic veneering, acrylic veneeringDental |
|||
Tensile Strength, Yield | 520 MPa @Strain 0.200 % |
75400 psi @Strain 0.200 % |
after porcelain firing |
Wieland Porta Geo Ti PFM Alloy Gold-platinum ceramic alloyApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneering, acrylic veneeringDental |
|||
Tensile Strength, Yield | 520 MPa @Strain 0.200 % |
75400 psi @Strain 0.200 % |
after porcelain firing |
Wieland Porta SMK 82 PFM Alloy Gold-palladium ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials, ceramic veneering, acrylic veneeringDental |
|||
Tensile Strength, Yield | 520 MPa @Strain 0.200 %, Thickness 127 - 152.4 mm |
75400 psi @Strain 0.200 %, Thickness 5.00 - 6.000 in |
Typical Strength |
Constellium Alumold® 500 Rolled Aluminum The Alumold® 500 alloy has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important prop.. |
|||
Tensile Strength, Yield | 520 MPa @Strain 0.200 %, Thickness 25.0 - 40.0 mm |
75400 psi @Strain 0.200 %, Thickness 0.984 - 1.57 in |
Typical Strength |
Constellium Fortal® Aluminum Alloy Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m.. |