Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 75400 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 520 MPa

@Strain 0.200 %,
Temperature 250 °C
>= 75400 psi

@Strain 0.200 %,
Temperature 482 °F
ThyssenKrupp N-A-XTRA® 620 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..
Tensile Strength, Yield 520 MPa

@Strain 0.200 %
75400 psi

@Strain 0.200 %
after porcelain firing
Wieland Duo Pal 6 PFM Alloy
Palladium-base ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials, ceramic veneering, acrylic veneeringDental
Tensile Strength, Yield 520 MPa

@Strain 0.200 %
75400 psi

@Strain 0.200 %
hardened
Wieland Duo Pal 6 PFM Alloy
Palladium-base ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials, ceramic veneering, acrylic veneeringDental
Tensile Strength, Yield 520 MPa

@Strain 0.200 %
75400 psi

@Strain 0.200 %
after porcelain firing
Wieland Porta Geo Ti PFM Alloy
Gold-platinum ceramic alloyApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneering, acrylic veneeringDental
Tensile Strength, Yield 520 MPa

@Strain 0.200 %
75400 psi

@Strain 0.200 %
after porcelain firing
Wieland Porta SMK 82 PFM Alloy
Gold-palladium ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials, ceramic veneering, acrylic veneeringDental
Tensile Strength, Yield 520 MPa

@Strain 0.200 %,
Thickness 127 - 152.4 mm
75400 psi

@Strain 0.200 %,
Thickness 5.00 - 6.000 in
Typical Strength
Constellium Alumold® 500 Rolled Aluminum
The Alumold® 500 alloy has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important prop..
Tensile Strength, Yield 520 MPa

@Strain 0.200 %,
Thickness 25.0 - 40.0 mm
75400 psi

@Strain 0.200 %,
Thickness 0.984 - 1.57 in
Typical Strength
Constellium Fortal® Aluminum Alloy
Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m..
Copyright © lookpolymers.com All Rights Reserved