Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 56.0 MPa @Temperature 300 °C |
>= 8120 psi @Temperature 572 °F |
|
PEAK Werkstoff DISPAL S541 Aluminum Alloy, AlMg6Mn4SiTiZr, Condition F Information provided by PEAK Werkstoff GmbH |
|||
Tensile Strength, Yield | 56.0 MPa @Temperature 982 °C |
8120 psi @Temperature 1800 °F |
ASTM E8 |
ATI Allegheny Ludlum 309S Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Tensile Strength, Yield | 56.0 MPa @Temperature 982 °C |
8120 psi @Temperature 1800 °F |
ASTM E8 |
ATI Allegheny Ludlum 310S Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |