Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 620 MPa

@Strain 0.200 %
>= 89900 psi

@Strain 0.200 %
H1150 Condition - 620°C
Latrobe Lescalloy® 13-8 Mo VIM-VAR Precipitation Hardening Stainless Steel
Lescalloy 13-8 Mo VIM-VAR is a precipitation hardening martensitic stainless steel offering excellent fracture toughness and transverse mechanical properties coupled with the resistance to stress-co..
Tensile Strength, Yield >= 620 MPa

@Thickness 65.0 mm
>= 89900 psi

@Thickness 2.56 in
ThyssenKrupp N-A-XTRA® M 620 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..