Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 620 MPa @Strain 0.200 % |
>= 89900 psi @Strain 0.200 % |
H1150 Condition - 620°C |
Latrobe Lescalloy® 13-8 Mo VIM-VAR Precipitation Hardening Stainless Steel Lescalloy 13-8 Mo VIM-VAR is a precipitation hardening martensitic stainless steel offering excellent fracture toughness and transverse mechanical properties coupled with the resistance to stress-co.. |
|||
Tensile Strength, Yield | >= 620 MPa @Thickness 65.0 mm |
>= 89900 psi @Thickness 2.56 in |
|
ThyssenKrupp N-A-XTRA® M 620 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |