Tensile Strength, Yield 547 MPa

@Strain 0.200 %,
Temperature 600 °C
79300 psi

@Strain 0.200 %,
Temperature 1110 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed, Age-hardened
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Tensile Strength, Yield 547 MPa

@Temperature 71.0 °C
79300 psi

@Temperature 160 °F
Hexcel® HexPly® F155 Epoxy Resin, K285 Kevlar Fabric
Information provided by HexCel
Tensile Strength, Yield 547 MPa

@Strain 0.200 %,
Temperature 600 °C
79300 psi

@Strain 0.200 %,
Temperature 1110 °F
Special Metals NIMONIC® alloy 91 Ni-Cr-Co Alloy
NIMONIC® alloy 91 is a wrought nickel-chromium-cobalt based alloy strengthened by additions of aluminum and titanium.This alloy is a modification of NIMONIC alloy 90, but has an increased chromium ..