Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.00409 - 0.00441 MPa-m/sec | 117 - 126 psi-ft/min | 3 m/min |
Polikim EFALON® B-40 PTFE, 40% Bronze Filled Bronze-filled Efalon® (PTFE) has better heat insulation, less thermal expansion, higher wear resistance properties and less deformation under load compared to virgin Efalon®. Applications: bearing.. |
|||
Limiting Pressure Velocity | 0.00409 - 0.00441 MPa-m/sec | 117 - 126 psi-ft/min | 30 m/min |
Polikim EFALON® C-15 PTFE, 15% Glass Filled C15 and C25 have less thermal expansion, higher wear resistance and less deformation under load compared to virgin Efalon® (PTFE). Applications: Seals, Seal rings, gaskets, valve sets, piston rings.. |
|||
Limiting Pressure Velocity | 0.00409 - 0.00654 MPa-m/sec | 117 - 187 psi-ft/min | 30 m/min |
Polikim EFALON® K-25 PTFE, 25% Carbon Filled K25 and K35 have less thermal expansion, higher wear resistance, less deformation under load properties compared to virgin Efalon® (PTFE). Applications: Bearings, piston rings, gaskets, seal rings... |
|||
Limiting Pressure Velocity | 0.00409 - 0.00654 MPa-m/sec | 117 - 187 psi-ft/min | 30 m/min |
Polikim EFALON® K-35 PTFE, 35% Carbon Filled K25 and K35 have less thermal expansion, higher wear resistance, less deformation under load properties compared to virgin Efalon® (PTFE). Applications: Bearings, piston rings, gaskets, seal rings... |