Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.00409 - 0.00441 MPa-m/sec
117 - 126 psi-ft/min
3 m/min
Polikim EFALON® B-40 PTFE, 40% Bronze Filled
Bronze-filled Efalon® (PTFE) has better heat insulation, less thermal expansion, higher wear resistance properties and less deformation under load compared to virgin Efalon®. Applications: bearing..
Limiting Pressure Velocity 0.00409 - 0.00441 MPa-m/sec
117 - 126 psi-ft/min
30 m/min
Polikim EFALON® C-15 PTFE, 15% Glass Filled
C15 and C25 have less thermal expansion, higher wear resistance and less deformation under load compared to virgin Efalon® (PTFE). Applications: Seals, Seal rings, gaskets, valve sets, piston rings..