Mechanical Properties Metric English Comments
Limiting Pressure Velocity 0.140 MPa-m/sec
4000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP Acetron® MD Metal-detectable Copolymer Acetal (ASTM Product Data Sheet)
Low moisture absorption High strength, stiffness Easy to machine No centerline porosity in Acetron® GP Many formulation options: Copolymer, Homopolymer, PTFE filled, and Internally lubricated/enha..
Limiting Pressure Velocity 0.140 MPa-m/sec
4000 psi-ft/min
at 0.1 m/s unlubricated
Quadrant EPP Ertalon® 6XAU+ PA 6, heat stabilized, cast (ISO Data)
Ertalon 6 XAU+ is a heat stabilized cast nylon grade with a very dense and highly crystalline structure. Compared with conventional extruded or cast nylons, Ertalon 6 XAU+ offers superior heat agein..
Limiting Pressure Velocity 0.140 MPa-m/sec
4000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP TIVAR® 88 ESD UHMW-PE, Premium Glass Filled, Crosslinked Electro Static Dissipative Lining Material (ASTM Product Data Sheet)
Limiting Pressure Velocity 0.140 MPa-m/sec
4000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP TIVAR® 88 UHMW-PE, Premium Glass Filled, Crosslinked Lining Material (ASTM Product Data Sheet)
Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic fl..
Limiting Pressure Velocity 0.140 MPa-m/sec
4000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP TIVAR® 88 W/BurnGuard, Flame Retardant Lining Material (ASTM Product Data Sheet)
Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic fl..
Limiting Pressure Velocity 0.140 MPa-m/sec
4000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP TIVAR® 88-2 ESD Black, Premium Lubricant Filled, Lower COF, Electro Static Dissipative Lining Material (ASTM Product Data Sheet)
Limiting Pressure Velocity 0.140 MPa-m/sec
4000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP TIVAR® 88-2 UHMW-PE, Premium Lubricant Filled Lining Material (ASTM Product Data Sheet)
Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic f..
Limiting Pressure Velocity 0.140 MPa-m/sec
4000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP TIVAR® DrySlide UHMW-PE, Lubricant Filled, Electro Static Dissipative, UV Stabilized (ASTM Product Data Sheet)
Limiting Pressure Velocity 0.140 MPa-m/sec
4000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP TIVAR® Oil Filled UHMW-PE FDA/USDA Oil-Filled UHMW-PE (ASTM Product Data Sheet)
Limiting Pressure Velocity 0.140 MPa-m/sec
4000 psi-ft/min
4:1 safety factor; QTM 55007
Quadrant EPP Duratron® PAI T4503 Compression Molded, Polyamide-imide, Eelectrical Grade (ASTM Product Data Sheet)
Limiting Pressure Velocity 0.140 MPa-m/sec
4000 psi-ft/min
4:1 safety factor applied; QTM 55010
Quadrant EPP Semitron® CMP XL20 (ASTM Product Data Sheet)
Limiting Pressure Velocity 0.140 - 1.10 MPa-m/sec
4000 - 31400 psi-ft/min
Average value: 0.556 MPa-m/sec Grade Count:6