Quadrant EPP Ertalon® 6XAU+ PA 6, heat stabilized, cast (ISO Data)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Cast
Manufacturer Quadrant Engineering Plastics Products
Trade Name Ertalon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Ertalon® 6XAU+ PA 6, heat stabilized, cast (ISO Data).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ertalon 6 XAU+ is a heat stabilized cast nylon grade with a very dense and highly crystalline structure. Compared with conventional extruded or cast nylons, Ertalon 6 XAU+ offers superior heat ageing performance in air (much better resistance to thermal-oxidative degradation), allowing 15-30 °C higher continuously allowable service temperatures. Ertalon 6 XAU+ is particularly recommended for bearings and other mechanical parts subject to wear which are operating in air for long periods of time at temperatures over 60 °C. High mechanical strength, stiffness, hardness and toughness Good fatigue resistance High mechanical damping ability Good sliding properties Excellent wear resistance Good electrical insulating properties Good resistance to high energy radiation (gamma- and X-rays) Good machinability
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183-1
Moisture Absorption at Equilibrium 2.2 %
2.2 %
50% RH
Water Absorption at Saturation 6.5 %
6.5 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 87
87
ISO 2039-2
Hardness, Shore D 80
80
Ball Indentation Hardness 165 MPa
23900 psi
ISO 2039-1
Tensile Strength 86.0 MPa
12500 psi
at Yield; ISO 527-1/-2
Elongation at Break 25 %
25 %
ISO 527-1/-2
Elongation at Yield 5.0 %
5.0 %
ISO 527-1/-2
Tensile Modulus 3.50 GPa
508 ksi
ISO 527-1/-2
Flexural Strength 122 MPa
17700 psi
Flexural Modulus 3.31 GPa
480 ksi
Compressive Strength 34.0 MPa

@Strain 1 %
4930 psi

@Strain 1 %
ISO 604
64.0 MPa

@Strain 2 %
9280 psi

@Strain 2 %
ISO 604
93.0 MPa

@Strain 5 %
13500 psi

@Strain 5 %
ISO 604
K Factor (ISO) 11 µm/km
11 µm/km
Charpy Impact Unnotched NB
NB
ISO 179-1/1eU
Charpy Impact, Notched 0.300 J/cm²
1.43 ft-lb/in²
ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.40 - 0.60
0.40 - 0.60
Limiting Pressure Velocity 0.0900 MPa-m/sec
2570 psi-ft/min
at 1 m/s unlubricated
0.140 MPa-m/sec
4000 psi-ft/min
at 0.1 m/s unlubricated
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C

@Temperature 23.0 - 100 °C
50.0 µin/in-°F

@Temperature 73.4 - 212 °F
Thermal Conductivity 0.290 W/m-K
2.01 BTU-in/hr-ft²-°F
Melting Point 215 °C
419 °F
DSC, 10°C/min.; ISO 11357-1/-3
Maximum Service Temperature, Air 105 °C
221 °F
Continuous; 20,000 h
120 °C
248 °F
Continuous; 5,000 h
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
Oxygen Index 25 %
25 %
ISO 4589-1/-2
Electrical Properties Metric English Comments
Volume Resistivity >= 1.0e+14 ohm-cm
>= 1.0e+14 ohm-cm
IEC 60093
Surface Resistivity per Square >= 1.0e+13 ohm
>= 1.0e+13 ohm
IEC 60093
Dielectric Constant 3.6

@Frequency >=100000 Hz
3.6

@Frequency >=100000 Hz
IEC 60250
Dielectric Strength 29.0 kV/mm
737 kV/in
Dissipation Factor 0.015

@Frequency 100000 Hz
0.015

@Frequency 100000 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Compliance Properties Metric English Comments
3A-Dairy No
No
European Food 1935/2004 No
No
FDA No
No
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Unacceptable
Unacceptable
Acids, Weak Limited
Limited
Alcohols Limited
Limited
Alkalies, Strong (pH 11-14) Unacceptable
Unacceptable
Alkalies, Weak Limited
Limited
Chlorinated Solvents Limited
Limited
Continuous Sunlight Limited
Limited
Hot Water / Steam Limited
Limited
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Acceptable
Acceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Acceptable
Acceptable
Users viewing this material also viewed the following: