Polymer Property : Limiting Pressure Velocity = 42800 psi-ft/min Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Limiting Pressure Velocity 1.50 MPa-m/sec
42800 psi-ft/min
at 0.5 m/s
Shell Carilon® DA6P2L10 Polyketone, High Performance Lubricated Injection Molding Grade  (discontinued **)
Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DA6P2L10 is a high-performance lubricated injection molding grade with mechanical properties which ..
Limiting Pressure Velocity 1.50 MPa-m/sec
42800 psi-ft/min
Kuraray Genestarâ„¢ G1352A-M41 Nylon, 35% Glass Filled
Low friction reinforced injection grade.Main Features:Low friction coefficientAbrasion resistanceExamples of applications:Friction and wear applicationGear and wheel
Limiting Pressure Velocity 1.50 MPa-m/sec
42800 psi-ft/min
Trelleborg Sealing Solutions Turcite® TX Self-Lubricating Thermoplastic Rod
Red color. Turcite® TX is engineered to handle moderate load, high speed applications. It exhibits an excellent surface finish when machined. It has a long service life and exceptionally low coe..