Trelleborg Sealing Solutions Turcite® TX Self-Lubricating Thermoplastic Rod

Category Polymer , Thermoplastic
Manufacturer Trelleborg Sealing Solutions (Smiths Group)
Trade Name Turcite®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Sealing Solutions Turcite® TX Self-Lubricating Thermoplastic Rod.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Red color. Turcite® TX is engineered to handle moderate load, high speed applications. It exhibits an excellent surface finish when machined. It has a long service life and exceptionally low coefficient of friction and high PV.General Turcite® information: Exhibit excellent wear resistance, durability, and no slip-stick under oscillating motion. Axial-loaded shafts benefit from reduced friction. Uses include transmissions, home appliances, bicycles, food processing equipment, exercise equipment, rotating displays, and caster assemblies.Informatiuon provided by Busak + Shamban, now Trelleborg Sealing Solutions.Busak+Shamban changed its name to Trelleborg Sealing Solutions in 2007.
Physical Properties Metric English Comments
Water Absorption 0.20 %
0.20 %
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 40.7 MPa
5900 psi
Elongation at Break 19 %
19 %
Coefficient of Friction 0.22
0.22
non-lubricated
K (wear) Factor 40.3 x 10-8 mm³/N-M
20.0 x 10-10 in³-min/ft-lb-hr
Limiting Pressure Velocity 1.50 MPa-m/sec
42800 psi-ft/min
Thermal Properties Metric English Comments
CTE, linear 93.6 µm/m-°C

@Temperature 20.0 °C
52.0 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 82.0 °C
180 °F
Continuous
95.0 °C
203 °F
Deflection Temperature with load unspecified
121 °C
250 °F
Intermittent