Polymer Property : Limiting Pressure Velocity = 47580 psi-ft/min Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Limiting Pressure Velocity 1.667 MPa-m/sec
47580 psi-ft/min
v = 200m/min
Wolf Kunststoff ZEDEX® ZX-410V7T A4T Polymer Alloy, Fiber Reinforced, Friction Modified
Main Characteristics: Fiber-reinforced; Friction-modified; Very high stiffness (higher than that of fiber-reinforced PEEK); Very low thermal expansion coefficient; Low friction; High wear resistance..