Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 10.7 MPa
1550 psi
at 2% offset; ASTM D882
ExxonMobil LD 051.LJ Shrink Film Resin  (discontinued **)
LD 051 blown film resins are designed for demanding heavy duty film applications, and combine excellent strength properties with outstanding processability. Used in heavy duty shipping bags and shr..
Film Tensile Strength at Yield, MD 10.7 MPa
1550 psi
at 2% offset; ASTM D882
ExxonMobil LD 051.LT Shrink Film Resin  (discontinued **)
LD 051 blown film resins are designed for demanding heavy duty film applications, and combine excellent strength properties with outstanding processability. Used in heavy duty shipping bags and shr..
Film Tensile Strength at Yield, MD 10.7 MPa
1550 psi
at 2% offset; ASTM D882
ExxonMobil LD 136.MV Packaging Film Resin  (discontinued **)
LD 136 series resins are homopolymer film resins with good clarity. They are suitable for processing in cast film equipment. Applications include food packaging, textile packaging, and other packa..
Film Tensile Strength at Yield, MD 10.7 MPa
1550 psi
at 2% offset; ASTM D882
ExxonMobil LD 136.NI Packaging Film Resin  (discontinued **)
LD 136 series resins are homopolymer film resins with good clarity. They are suitable for processing in cast film equipment. Applications include food packaging, textile packaging, and other packa..
Film Tensile Strength at Yield, MD 10.7 MPa
1550 psi
Dow DOWLEX™ 2045 Linear Low Density Polyethylene, Heavy Duty Film Grade
DOWLEX® 2045 Polyethylene resin is a premier film resin for heavy duty applications. It complies with U.S. FDA regulation 21 CFR 177.1520 (c) 3.2(a) for food contact applications. The regulation sh..
Film Tensile Strength at Yield, MD 10.7 MPa
1550 psi
Dow DOWLEX™ 2045A Linear Low Density Polyethylene, Blown Film Grade
DOWLEX® 2045A Polyethylene blown film extrusion resin is a premier film resin for heavy duty applications. It is utilized where improved thermal stability over a broader range of processing conditi..
Film Tensile Strength at Yield, MD 10.7 MPa
1550 psi
Dow DOWLEX™ 2056 Linear Low Density Polyethylene, Heavy Duty Film Grade
DOWLEX® 2056 Polyethylene resin is a premier polymer for heavy duty blown film applications. It is a low gel, high consistency polymer. It complies with U.S. FDA Regulation 21 CFR 177.1520 (c) 3.2 ..
Film Tensile Strength at Yield, MD 10.7 MPa
1550 psi
Dow DOWLEX™ 2056A Linear Low Density Polyethylene, Heavy Duty Film Grade
DOWLEX® 2056A Polyethylene is a premier polymer for heavy duty blown film applications. It is a low gel, high consistency polymer with improved thermal stability and is an outstanding choice for cr..
Film Tensile Strength at Yield, MD 10.7 MPa
1550 psi
ASTM D882
Dow DOWLEX™ 2070G Linear Low Density Polyethylene
High strength in food packaging applications Good processability at narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow
Film Tensile Strength at Yield, MD 10.7 MPa
1550 psi
Dow DOWLEX™ 2245A Linear Low Density Polyethylene, Heavy Duty Film Grade
DOWLEX® 2245A Polyethylene resin is a premier film resin for heavy duty applications. DOWLEX 2245A resin is used where improved thermal stability over a broad range of processing conditions is nece..
Film Tensile Strength at Yield, MD 10.7 MPa
1550 psi
Dow DOWLEX™ 2245D Linear Low Density Polyethylene, Heavy Duty Film Grade
DOWLEX® 2245D Polyethylene resin is a premier film resin for heavy duty applications. DOWLEX 2245D resin is used where improved thermal stability over a broad range of processing conditions is nece..
Film Tensile Strength at Yield, MD 10.7 MPa
1550 psi
ASTM D882
Dow FLEXOMER™ ETS-9066 NT 7, 0.8 mil Very Low Density Polyethylene (VLDPE) Resin
FLEXOMER™ ETS-9066 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, an..
Film Tensile Strength at Yield, MD 10.7 MPa
1550 psi
Dow LDPE 586A Low Density Polyethylene, Packaging Grade