Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 8.50 MPa
1230 psi
ASTM D 882
NOVA Chemicals Sclair® FP619-A Octene Copolymer LLDPE Film Resin
FP619-A complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, withou..
Film Tensile Strength at Yield, MD 8.48 MPa
1230 psi
at 2% offset; ASTM D882
ExxonMobil LL 1002.32 Blown Film Resin  (discontinued **)
LL1002 resins are butene LLDPE designed for blown film process, with good tensile and toughness properties.Information provided by ExxonMobil Chemical
Film Tensile Strength at Yield, MD 8.48 MPa
1230 psi
at 2% offset; ASTM D882
ExxonMobil LL 1002x74 Blown Film Resin  (discontinued **)
LL1002 resins are butene LLDPE designed for blown film process, with good tensile and toughness properties.Information provided by ExxonMobil Chemical
Film Tensile Strength at Yield, MD 8.48 MPa
1230 psi
at 2% offset; ASTM D882
ExxonMobil LL 1002x79 Blown Film Resin  (discontinued **)
LL1002 resins are butene LLDPE designed for blown film process, with good tensile and toughness properties.Information provided by ExxonMobil Chemical
Film Tensile Strength at Yield, MD 8.48 MPa
1230 psi
at 2% offset; ASTM D882
ExxonMobil Escorene® LD 767.MJ Cast and Compounding Film Resin  (discontinued **)
Escorene Ultra LD 767.MJ is a low gel 29.5% vinyl acetate copolymer designed for film and compounding applications.Information provided by ExxonMobil Chemical
Film Tensile Strength at Yield, MD 8.50 MPa
1230 psi
ASTM D 882
NOVA Chemicals Surpass® FPs016-C Octene sLLDPE Film Resin
FPs016-C complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem..
Film Tensile Strength at Yield, MD 8.48 MPa
1230 psi
ASTM D882
ExxonMobil LL 1002.09 Blown Film Resin
Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat..
Film Tensile Strength at Yield, MD 8.48 MPa
1230 psi
at 2% offset; ASTM D882
ExxonMobil LL 1002x75 Blown Film Resin
Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat..
Film Tensile Strength at Yield, MD 8.50 - 12.0 MPa
1230 - 1740 psi
Average value: 9.49 MPa Grade Count:28
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Octene, Film
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Octene, Film". Each property range of values reported is minimum..