Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NOVA Chemicals Sclair® FP619-A Octene Copolymer LLDPE Film Resin

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE)/Octene, Film
Manufacturer NOVA Chemicals
Trade Name Sclair®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Sclair® FP619-A Octene Copolymer LLDPE Film Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FP619-A complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without temperature or food-type restrictions, subject to technical suitabilityNOVA Chemicals' polyethylene resins are chemically and biologically inert.Features: Exceptional toughness, Low gel levelApplications: Cast film, Co-extrusion and laminationFilm properties are typical of cast film extruded at a melt temperature of 500°F, and a line speed of 800 ft/min.
Physical Properties Metric English Comments
Density 0.919 g/cc
0.0332 lb/in³
ASTM D 792
Thickness 20.0 microns
0.787 mil
Melt Flow 5.9 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.9 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 8.50 MPa
1230 psi
ASTM D 882
Film Tensile Strength at Yield, TD 8.30 MPa
1200 psi
ASTM D 882
Film Elongation at Break, MD 472 %
472 %
ASTM D 882
Film Elongation at Break, TD 647 %
647 %
ASTM D 882
Elmendorf Tear Strength MD 320 g
320 g
ASTM D 1922
Elmendorf Tear Strength TD 520 g
520 g
ASTM D 1922
Elmendorf Tear Strength, MD 16.0 g/micron
406 g/mil
ASTM D 1922
Elmendorf Tear Strength, TD 26.0 g/micron
660 g/mil
Dart Drop Test 131 g
0.289 lb
7; ASTM D 1709/A
Film Tensile Strength at Break, MD 28.3 MPa
4100 psi
ASTM D 882
Film Tensile Strength at Break, TD 22.2 MPa
3220 psi
ASTM D 882
1% Secant Modulus, MD 116 MPa
16800 psi
ASTM D 882
1% Secant Modulus, TD 135 MPa
19600 psi
ASTM D 882
Optical Properties Metric English Comments
Haze 1.0 %
1.0 %
ASTM D 1003
Gloss 91.5 %
91.5 %
at 45°; ASTM D 2457
Descriptive Properties Value Comments
Low Friction Puncture (J/mm) 52
NOVA Chemicals Test Method