Polymer Property : Film Tensile Strength at Yield, MD = 13900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 95.8 MPa

@Strain >=5.00 %
13900 psi

@Strain >=5.00 %
ASTM D882A
DuPont Teijin Films Melinex® 306 Polyester Film, 300 Gauge
Melinex® 306 is a clear, smooth pretreated polyester film. Melinex® 306 is produced from a lightly filled polymer, giving it a very smooth surface. The two side chemical coating provides adhesion ..
Film Tensile Strength at Yield, MD 95.8 MPa

@Strain >=5.00 %
13900 psi

@Strain >=5.00 %
ASTM D882A
DuPont Teijin Films Melinex® 606 Polyester Film, 300 Gauge
Melinex® 606 is a very smooth two-side coated polyester film designed specifically for high density floppy disks.Also available in 285 GaugeInformation provided by DuPont.
Film Tensile Strength at Yield, MD 95.8 MPa

@Strain >=5.00 %
13900 psi

@Strain >=5.00 %
ASTM D882A
DuPont Teijin Films Mylar® ADS Polyester Film, 300 Gauge
Mylar® ADS is a heat stabilized, low shrinkage film with good web handling properties. Approvals: UL 94 VTM-2 - for 92 - 500 gauge (0.023 - 0.13mm)Also available in 285 GaugeInformation provided by..