Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 9.818 MPa
1424 psi
ASTM D882
Dow ELITE™ 5400G Enhanced Polyethylene Resin
™ 5400G is a copolymer produced via INSITE™ Technology from Dow Plastics. It offers a unique combination of low seal initiation, moderate stiffness and low blocking tendencies for good performanc..
Film Tensile Strength at Yield, MD 9.818 MPa
1424 psi
ASTM D882
Dow TUFLIN™ HSE-7002 NT 7 Linear Low Density Polyethylene Resin
Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HSE-7002 NT 7 is an ethylene-hexene-1 copolymer, design..