Film Tensile Strength at Yield, MD 9.93 MPa
1440 psi
ASTM D882
Dow AFFINITY™ PL 1850G Polyolefin Plastomer (POP)
AFFINITY™ PL 1840G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed to provide blown and cast film products with low temperature sealability, excellent optics and g..
Film Tensile Strength at Yield, MD 9.90 MPa
1440 psi
Dow DOWLEX™ NG 2085 Linear Low Density Polyethylene, Ethylene-Octene Copolymer
Next Generation DOWLEX® NG 2085 resin is an ethylene-octene copolymer offering superior impact and tensile strength for down-gauged consumer liner film applications. It complies with U.S. FDA regul..