Film Tensile Strength at Yield, MD 17.0 MPa
2470 psi
ISO 527-3
Polimeri Europa Flexirene® CM 50 Butene Copolymer Linear Low Density Polyethylene
Flexirene CM 50 is a butene copolymer with medium density (C4-LLDPE), with antioxidants, suitable for cast film extrusion.Main Applications: Flexirene CM 50 is a highly stiff product and it is reco..
Film Tensile Strength at Yield, MD 17.0 MPa
2470 psi
ASTM D882
NOVA Chemicals Sclair® 14G Butene LMDPE Film Resin
Film Properties. Features: Low gel, good opacity, easy processability.Applications: Overwrap film.Data provided by the manufacturer.
Film Tensile Strength at Yield, MD 17.0 MPa
2470 psi
ASTM D882
ExxonMobil Escorene® LD-103 LDPE Industrial Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer industrial film resin with excellent toughness. LD-103 has a low melt index which gives excellent impact strength and melt strength o..
Film Tensile Strength at Yield, MD 17.0 MPa
2470 psi
ASTM D882
NOVA Chemicals Sclair® 14B3 Butene LMDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, good clarity, heat resistance and barrier properties.Applications: Lamination, co-extrusion.Data provided by the manufacturer.
Film Tensile Strength at Yield, MD 17.0 MPa
2470 psi
ASTM D882
NOVA Chemicals Sclair® 14L1 Octene LMDPE Film Resin  (discontinued **)
Low gel, Good clarity, Excellent sealing characteristicsApplications: Lamination, Co-extrusionAdditives: Process stabilizer, polymer process aidFilm properties are typical of blown film extruded at ..
Film Tensile Strength at Yield, MD 17.0 MPa
2470 psi
UBE 7024B Five Layer Film
Specialties: High transparencyGood thermoform-abilityLow W.V.T.R High shrink-abilityLower extrusion temperatureProcessing: Best match for co-extrusion with EVOH resins.Typical Applications: Cereal ..
Film Tensile Strength at Yield, MD 17.0 MPa
2470 psi
ASTM D882
NOVA Chemicals Novapol® TF-0242-E Hexene LLDPE Film Resin  (discontinued **)
Excellent stiffness and glossApplications: Diaper back sheet, BlendingFilm properties are typical of film extruded at 270°C.Information provided by NOVA Chemicals.
Film Tensile Strength at Yield, MD 17.0 MPa
2470 psi
ASTM D882
NOVA Chemicals Sclair® 14B1 Butene LMDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, good clarity, heat resistance and barrier properties.Applications: Lamination, co-extrusion.Data provided by the manufacturer.