Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Film Tensile Strength at Yield, MD = 1700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 11.7 MPa
1700 psi
at 2% offset; ASTM D882
ExxonMobil Exceed™ 1327CA Blown Film Resin  (discontinued **)
Exceed 1327CA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1327CA resin have outstanding tensile, impact strength and puncture. These superi..
Film Tensile Strength at Yield, MD 11.7 MPa
1700 psi
ASTM D882
Westlake LF1050 Butene Linear Low Density Polyethylene
Westlake LF1050 is a butene LLDPE with high stiffness suitable for cast film extrusion. This material can be used at 100% or as blending stock with LDPE or MDPE.Application/UsesCast film extrusionPr..
Film Tensile Strength at Yield, MD 11.7 MPa
1700 psi
ASTM D882
ExxonMobil LDPE LD 165BW1 Low Density Polyethylene Resin (European Grade)
Product Description: LD 165 series are LDPE grades, offering high strength combined with medium optical properties.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoTherm..
Film Tensile Strength at Yield, MD 11.7 MPa
1700 psi
at 2% offset; ASTM D882
ExxonMobil LL 3201.36 Premium High Strength Film Resin
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al..
Film Tensile Strength at Yield, MD 11.7 MPa
1700 psi
ASTM D882
ExxonMobil LL 3201.69 Premium High Strength Film Resin
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al..
Film Tensile Strength at Yield, MD 11.7 MPa
1700 psi
ASTM D882
ExxonMobil LLDPE LL 3201.36 Linear Low Density Polyethylene Resin
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al..
Film Tensile Strength at Yield, MD 11.7 MPa
1700 psi
ASTM D882
ExxonMobil LLDPE LL 3201.69 Linear Low Density Polyethylene Resin
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al..
Film Tensile Strength at Yield, MD 11.7 MPa
1700 psi
Dow DOWLEX™ 2032 Linear Low Density Polyethylene, Blown Film Grade
DOWLEX® 2032 Polyethylene resin is a general purpose liner resin having improved thermal stability over a broad range of processing conditions. It is an outstanding choice for thin gauge, medium st..
Film Tensile Strength at Yield, MD 11.7 MPa
1700 psi
Dow DOWLEX™ 2101 Linear Low Density Polyethylene, Blown Film Grade
DOWLEX® 2101 Polyethylene resin, a general purpose blown film extrusion resin, is an excellent choice for high speed, thin gauge film applications. It contains medium levels of both slip additive a..
Film Tensile Strength at Yield, MD 11.7 MPa
1700 psi
Dow LDPE 534A Low Density Polyethylene, Blown Film Grade
DOW LDPE 534A resin, is a general purpose blown film extrusion resin with excellent drawdown and processability for packaging applications. It contains medium levels of both slip additive and antibl..
Film Tensile Strength at Yield, MD 11.7 MPa
1700 psi
Dow LDPE 681I Low Density Polyethylene, Liner Film Grade
DOW LDPE 681I resin is a barefoot general purpose medium duty liner film resin for packaging applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food contact appl..
Copyright © lookpolymers.com All Rights Reserved