Material Notes:
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, along with good drawdown capability, permit usage in many demanding packing applications.Availability: Latin America, North America and South America Additive: Antiblock: 5000 ppmSlip: NoProcessing Aid: Yes Thermal Stabilizer: YesApplications: Freezer FilmGrocery SacksHeavy Duty BagsMerchandise BagsInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.926 g/cc
0.0335 lb/in³
ExxonMobil method
Melt Flow 0.80 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 5000 ppm
5000 ppm
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 11.7 MPa
1700 psi
ASTM D882
Film Tensile Strength at Yield, TD 13.8 MPa
2000 psi
ASTM D882
Film Elongation at Break, MD 510 %
510 %
ASTM D882
Film Elongation at Break, TD 810 %
810 %
ASTM D882
Puncture Energy 2.94 J
2.17 ft-lb
ExxonMobil Method
Elmendorf Tear Strength MD 140 g
140 g
ASTM D1922
Elmendorf Tear Strength TD 780 g
780 g
ASTM D1922
Dart Drop Test 110 g
0.243 lb
ASTM D1709A
Film Tensile Strength at Break, MD 61.4 MPa
8900 psi
ASTM D882
Film Tensile Strength at Break, TD 48.3 MPa
7000 psi
ASTM D882
1% Secant Modulus, MD 234 MPa
34000 psi
ASTM D882
1% Secant Modulus, TD 283 MPa
41000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 257 °C
<= 495 °F
Peak Melting Point; ExxonMobil method
Optical Properties Metric English Comments
Haze 11 %
11 %
ASTM D1003
Gloss 57 %
57 %
45°; ASTM D2457
Descriptive Properties Value Comments
Puncture Force 10 lbf
ExxonMobil Method
Users viewing this material also viewed the following: