Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 13.0 MPa
1890 psi
ASTM D882
SABIC 318B Linear Low Density Polyethylene for Cast Film
Product Description: 318B is a Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high processing temperatures u..
Film Tensile Strength at Yield, MD 13.0 MPa
1890 psi
ASTM D882
SABIC 6318B Linear Low Density Polyethylene for Cast Film
Product Description: 6318B is a hexene copolymer Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high process..
Film Tensile Strength at Yield, MD 13.0 MPa
1890 psi
ASTM D882
SABIC 726 Series Linear Low Density Polyethylene for Blown Film
Product Description: 726 series resins are fractional index Linear Low Density Polyethylene grades suitable for blown film applications. Films produced using these resins give a relatively higher ..
Film Tensile Strength at Yield, MD 13.0 MPa
1890 psi
ISO 527
Premix Thermoplastics PRE-ELEC® CP 1319
PRE-ELEC CP 1319 is a conductive thermoplastic compound based on EVA. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC CP 1319 ..
Film Tensile Strength at Yield, MD 13.0 MPa
1890 psi
ASTM D882
NOVA Chemicals Novapol® TF-Y826-CP Hexene LLDPE Film Resin
Film Properties. Features: Good stiffness, intended for narrow die gaps, high strength and toughness.Applications: Industrial bags, industrial packaging.Data provided by the manufacturer.
Film Tensile Strength at Yield, MD 13.0 MPa
1890 psi
ASTM D882
ExxonMobil Escorene® LL-1108 LLDPE Film/Sandwich Bag Resin, 0.6 mil film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.An LLDPE blown film resin formulated with high slip, medium antiblock and processing aid for narrow die gap extrusion. Films made from LL-1108 have..
Film Tensile Strength at Yield, MD 13.0 MPa
1890 psi
ASTM D882
NOVA Chemicals Novapol® TF-Y826-D Hexene LLDPE Film Resin
Film Properties. Features: High strength and toughness, excellent puncture resistance, good stiffness and machinability.Applications: Premium trash bags, bags-on-roll.Data provided by the manufactu..
Film Tensile Strength at Yield, MD 13.0 MPa
1890 psi
ASTM D882
ExxonMobil Escorene® LD-117 MDPE Blown Overwrap Film Resin, Tough  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity and excellent stiffness. Film made from LD-117 can be used in overwrap applications and in push-through ..
Film Tensile Strength at Yield, MD 13.0 MPa
1890 psi
ASTM D882-02
Ipiranga Petrochem LB 0117 LLDP
IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba..
Film Tensile Strength at Yield, MD 13.0 MPa
1890 psi
ASTM D882-02
Ipiranga Petrochem LB 0120 BS LLDP
IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba..
Film Tensile Strength at Yield, MD 13.0 MPa
1890 psi
ISO R527-1
Iran Petrochemical (PCC) 2102TX00 Low Density Polyethylene
LDPE 2102TX00 GP filmIt is used in wide range of widths and thicknesses e.g. for punches, bags, liners and lamination film.Information provided by Iran Petrochemical Commercial Co.
Film Tensile Strength at Yield, MD 13.0 MPa
1890 psi
ISO R527-1
Iran Petrochemical (PCC) 2404TC47 Low Density Polyethylene
LDPE 2404TC47 Light duty FilmIt is used for very thin films requiring good optical properties for general packaging applications e.g. covering film with very low blocking tendency.Information provi..
Film Tensile Strength at Yield, MD 13.0 MPa
1890 psi
ISO R527-1
Iran Petrochemical (PCC) 2602TH00 Low Density Polyethylene
LDPE 2602TH00 high clarity film Applications: film, underblankets and films for medical applications.Information provided by Iran Petrochemical Commercial Co.
Film Tensile Strength at Yield, MD 13.0 MPa
1890 psi
ISO 527
Iran Petrochemical (PCC) LF0250/KJ Low Density Polyethylene
LF0250/KJ is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties.Application: packaging films.Information provid..
Film Tensile Strength at Yield, MD 13.0 MPa
1890 psi
ASTM D882
Iran Petrochemical (PCC) LL22501 Linear Low Density Polyethylene
22501 is a high stiffness LLDPE blown film grade designed for applications requiring good optical properties even at low extrusion temperature. This resin combines ease of processing with low gels a..
Film Tensile Strength at Yield, MD 13.0 MPa
1890 psi
Dow DOWLEX™ 2071 Linear Low Density Polyethylene
DOWLEX® 2071 Polyethylene resin is a linear low density polyethylene resin specifically designed for the manufacture of high strength, thin gauge films for use in applications such as grocery sacks..
Film Tensile Strength at Yield, MD 13.0 MPa
1890 psi
at 2% offset; ASTM D882
ExxonMobil LL 3201.22 Premium High Strength Film Resin  (discontinued **)
LL 3201 resins are hexene copolymer LLDPE film resins. Films produced from these resins have excellent tensile, toughness and stiffness properties. These strength properties, along with good drawdow..
Film Tensile Strength at Yield, MD 13.0 MPa
1890 psi
ASTM D882
NOVA Chemicals Novapol® TF-Y529-BP Hexene LLDPE  (discontinued **)
Puncture value is 50 J/mm. Hexene LLDPE. Excellent puncture resistance, good stiffness and machinability, and good tensile properties. Additive Package: High slip and antiblock, process aid.Applic..
Film Tensile Strength at Yield, MD 13.0 MPa
1890 psi
ASTM D882
NOVA Chemicals Novapol® TF-Y826-BP Hexene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Good stiffness and machinability, intended for narrow die gaps, high strength and toughness.Applications: Grocery sacks, boutique bags, frozen food packaging.Data provide..