Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 13.8 MPa | 2000 psi | ASTM D882 |
ExxonMobil LD 117.85 Blown Overwrap Film Resin Product Description: LD 117.85 is a homopolymer film resin with good clarity and excellent stiffness. Film made from LD 117.85 resin can be used in overwrap applications and in push-through type pac.. |
|||
Film Tensile Strength at Yield, MD | 13.8 MPa | 2000 psi | ASTM D882 |
ExxonMobil LDPE LD 117.85 Low Density Polyethylene Resin Product Description: LD 117.85 is a homopolymer film resin with good clarity and excellent stiffness. Film made from LD 117.85 resin can be used in overwrap applications and in push-through type pac.. |
|||
Film Tensile Strength at Yield, MD | 13.8 MPa | 2000 psi | ASTM D882 |
Dow DOWLEX™ 2025G Linear Low Density Polyethylene DOWLEX™ 2025G is a medium modulus resin with excellent toughness properties designed for thin film applications.Information provided by Dow |